发明名称 LOW-SHRINKAGE META-TYPE WHOLLY AROMATIC POLYAMIDE FIBER AND METHOD FOR PRODUCING THE SAME
摘要 <P>PROBLEM TO BE SOLVED: To provide a low-shrinkage meta-type wholly aromatic polyamide fiber having a low heat shrinkage percentage at a high temperature. Ž<P>SOLUTION: The halogen atom-containing phosphoric acid ester-containing low-shrinkage meta-type wholly aromatic polyamide fiber having a maximum heat shrinkage percentage of ≤4.0%, a tensile strength of ≥2.8 cN/dtex and a limiting oxygen index (LOI value) of ≥28 is obtained by mixing a wholly aromatic polyamide with a specific amount of a halogen atom-containing phosphoric acid ester, drawing an obtained undrawn yarn in a specific ratio in wet-heat at one stage and performing a relaxing heat treatment in a specific ratio. Ž<P>COPYRIGHT: (C)2010,JPO&INPIT Ž
申请公布号 JP2010150681(A) 申请公布日期 2010.07.08
申请号 JP20080327445 申请日期 2008.12.24
申请人 TEIJIN TECHNO PRODUCTS LTD 发明人 YAMAUCHI HIROSUKE
分类号 D01F6/90;D02J1/22 主分类号 D01F6/90