发明名称 SLURRY PHASE POLYMERISATION PROCESS
摘要 Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80wt% of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80wt% of a low molecular weight (LMW) polymer is made in suspension in a second reactor, wherein the ratio of the average activity in the LMW reactor to the average activity in the HMW reactor is from 0.25 and 1.5, where average activity in each reactor is defined as the rate of polyethylene produced in the reactor (kgPE/hr) /[ethylene concentration in the reactor (mol%) x residence time in the reactor (hours) x feed rate of catalyst into the reactor (g/hr)], residence time being defined as the mass of the polymer in the reactor (kg)/the output rate of polymer from the reactor (kg/hr), and wherein the volume of the second reactor is at least 10%, preferably at least 30% and more preferably at least 50% greater than the volume of the first reactor, and the ratio of length to diameter of the first reactor, L/D(l), is greater than that of the second reactor, L/D(2), and preferably at least 20% greater.
申请公布号 KR20100066476(A) 申请公布日期 2010.06.17
申请号 KR20107004737 申请日期 2008.08.29
申请人 INEOS MANUFACTURING BELGIUM NV 发明人 KOCH BENOIT;MARISSAL DANIEL;PARISEL MARC;WALWORTH BRENT R.
分类号 C08F2/00;C08F2/01;C08F10/02;C08L23/06 主分类号 C08F2/00
代理机构 代理人
主权项
地址