摘要 <p><P>PROBLEM TO BE SOLVED: To provide a mold flux for continuous casting which simultaneously satisfies the three of low fluorine concentration, high basicity and lubricity. <P>SOLUTION: In the mold flux for continuous casting, the main crystals crystallized out or precipitated in the mold flux solidified after temporal melting are Melilite as a complete solid solution between Gehlenite and Akermanite. Also, a part of calcium contained in the Melilite is replaced by strontium. A mold flux having reduced environmental contamination and hard to be involved in molten steel can be obtained, and which is applicable to wide casting conditions. <P>COPYRIGHT: (C)2010,JPO&INPIT</p>
申请公布号 JP2010125457(A) 申请公布日期 2010.06.10
申请号 JP20080299333 申请日期 2008.11.25
申请人 SUMITOMO METAL IND LTD 发明人 TSUKAGUCHI YUICHI
分类号 B22D11/108;C21C7/076 主分类号 B22D11/108