发明名称 |
Goldlegierung zum Aufbrennen von Porzellan fuer zahnaerztliche Zwecke |
摘要 |
A gold based alloy suitable for use in dental work comprises: .Au.80.0-90.0% .Pt.5.0-15.0% .In.0.1-2.0% .Sn.0.1-2.0% .Re.0.05-1.0% preferably 0.1-0.5% In addition, one or more of the following elements may be present within the ranges stated: .Pd.up to 5% .Ag.up to 5% .Cu.up to 1% .Zn.up to 0.5% .Ir.0.05-0.5% Heat treatments described are heating for 15 minutes at 800 or 950 DEG C. with an optional second step of 15 minutes at 500 DEG C. |
申请公布号 |
DE1183247(B) |
申请公布日期 |
1964.12.10 |
申请号 |
DE1962D038024 |
申请日期 |
1962.01.30 |
申请人 |
DEUTSCHE GOLD- UND SILBER-SCHEIDEANSTALT VORMALS ROESSLER |
发明人 |
WAGNER DR. EWALD;PRALOW DR. WALTER ERNST LUDWIG |
分类号 |
A61C13/00;A61C13/03;A61C13/083;A61K6/04;A61K6/06;C22C5/02 |
主分类号 |
A61C13/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|