PROBLEM TO BE SOLVED: To provide a two color resin molding that is formed of a thermoplastic resin, shows excellence in rigidity and an impact property, and is reduced in warp. SOLUTION: The thermoplastic resin molding 3 comprises a first layer (A)1 composed of a thermoplastic resin (component A), and a second layer (B)2 piled up on a part of at least one surface of the first layer (A). The second layer (B) is formed of the following resin compositions (i) to (iii), that is, (i) 40 to 100 wt.% of an aromatic polycarbonate resin (component B-1), (ii) 0 to 60 wt.% of a thermoplastic resin (component B-2) other than the component B-1, and (iii) 1 to 50 pts.wt., based on 100 pts.wt. of the sum of the component B-1 and component B-2, of a flat cross-sectional glass fiber (component B-3) having an average major axis of the fiber cross section of 10 to 50μm and an average ratio of the major axis to the minor axis (major axis/minor axis) of 1.5 to 8. COPYRIGHT: (C)2010,JPO&INPIT |