发明名称 DETECTION METHOD OF SIGNIFICANT SOLIDIFICATION DELAY CAUSED BY BULGING OF SHELL ON NARROW FACE SIDE
摘要 <P>PROBLEM TO BE SOLVED: To provide an innovative method to avoid breakout immediately below a casting mold more reliably than ever. Ž<P>SOLUTION: When casting medium carbon steel at a high velocity, the following method is applied to detect a significant solidification delay caused by bulging of the shell on the narrow face side. Namely, a thermal flux q(MW/m<SP>2</SP>) of each narrow face of mold is measured at a point respectively near the bottom end of the mold. When the thermal flux q(MW/m<SP>2</SP>) of at least either one of the narrow faces of the mold satisfies such a condition that a standard deviation σ(MW/m<SP>2</SP>) of the thermal flux q(MW/m<SP>2</SP>) for at least 5 second period is 0.04 or more, it is determined that significant solidification delay occurs. Then, it is preferable to take a recovering measure for the significant solidification delay. Ž<P>COPYRIGHT: (C)2010,JPO&INPIT Ž
申请公布号 JP2010089150(A) 申请公布日期 2010.04.22
申请号 JP20080264041 申请日期 2008.10.10
申请人 KOBE STEEL LTD 发明人 USHIO HAJIME
分类号 B22D11/16;B22D11/00 主分类号 B22D11/16
代理机构 代理人
主权项
地址