摘要 |
A hydrotalcite-like granular material having a grain size of 0.24 mm or larger is produced by drying a material that contains at least a hydrotalcite-like substance and that has a water content of 70% or lower at equal to or lower than a temperature at which the hydrotalcite-like substance is dehydrated of crystal water contained therein, preferably at 90° C. or higher and 110° C. or lower, such that the resulting hydrotalcite-like granular material has a water content of 10% or higher. In this manner, a hydrotalcite-like granular material that has a stable morphology and a high anion exchange performance and that can be produced at a low cost can be produced. |