摘要 |
<P>PROBLEM TO BE SOLVED: To provide a resin excellent in rigidity, weld strength and surface smoothness. Ž<P>SOLUTION: This glass-fiber reinforced polyamide resin composition includes (A) 95-80 mass% polyamide, (B) 5-20 mass% polyarylate resin, (C) 30-70 mass% glass-fiber based on a total amount of (A), (B) and (C), and (D) 0.05-4.0 pts.mass organic compound having at least two functional groups selected from the group consisting of epoxy, acid anhydride, oxazoline, carboxylic acid, amino and isocyanate groups per one molecule, based on 100 pts.mass of the total amount of (A), (B) and (C). Ž<P>COPYRIGHT: (C)2010,JPO&INPIT Ž
|