<p>Described is a method for forming an internal frame configured to receive a flat screen display. Aggressive partial annealing is applied to a hard temper 5182 aluminum alloy material having magnesium content greater than or equal to 3.0 wt. %. The material is partial annealed to an extent that the hard temper aluminum alloy is substantially softened with respect to its initial hardened temper while not exceeding the point where recrystallization occurs. An internal frame for a flat screen display is formed from the partial annealed aluminum alloy.</p>