发明名称 |
METHOD FOR MANUFACTURING TITANIUM OXIDE-CONTAINING SLAG |
摘要 |
<p>THE PRESENT INVENTION PROVIDES A METHOD FOR EFFICIENTLY MANUFACTURING A TITANIUM OXIDE- CONTAINING SLAG FROM A MATERIAL INCLUDING TITANIUM OXIDE AND IRON OXIDE, WHEREIN A REDUCTION OF TITANIUM DIOXIDE IS SUPPRESSED AND THE ELECTRIC POWER CONSUMPTION IS MINIMIZED. THE METHOD INCLUDES THE STEPS OF : HEATING A RAW MATERIAL MIXTURE INCLUDING TITANIUM OXIDE, IRON OXIDE, AND A CARBONACEOUS REDUCTANT, OR THE RAW MATERIAL MIXTURE FURTHER INCLUDING A CALCIUM OXIDE SOURCE, IN A REDUCING FURNACE (6); REDUCING THE IRON OXIDE IN THE MIXTURE TO FORM REDUCED IRON; FEEDING THE RESULTANT MIXTURE TO A HEATING MELTING FURNACE (9); HEATING THE RESULTANT MIXTURE IN THE HEATING MELTING FURNACE (9) TO MELT THE REDUCED IRON AND SEPARATE THE REDUCED IRON FROM A TITANIUM OXIDE-CONTAINING SLAG; AND DISCHARGING AND RECOVERING THE TITANIUM OXIDE-CONTAINING SLAG OUT OF THE FURNACE (9).</p> |
申请公布号 |
MY140955(A) |
申请公布日期 |
2010.02.12 |
申请号 |
MY2003PI03784 |
申请日期 |
2003.10.03 |
申请人 |
KABUSHIKI KAISHA KOBE SEIKO SHO (KOBE STEEL, LTD.) |
发明人 |
HIDETOSHI TANAKA;ITSUO MIYAHARA;HIROSHI UEMURA;TAKAO HARADA;HIROSHI SUGITATSU;ISAO KOBAYASHI |
分类号 |
C01G23/04;C21B5/02;C21B11/08;C21B13/00;C21B13/10;C21B13/14;C21B15/02;C21C5/54;C22B7/04;C22B34/12;F27B9/02 |
主分类号 |
C01G23/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|