摘要 |
PROBLEM TO BE SOLVED: To provide a multi-layered sintered slide member excellent in fatigue durability, load withstanding characteristics, and frictional wear characteristics even in applications where a high facial pressure over the allowable facial pressure is applied. SOLUTION: The multi-layered sintered slide member is composed of a backing metal and a porous sintered layer integrally diffusion-bonded to the backing metal and including 3-10 wt.% Sn, 10-30 wt.% Ni, 0.5-4 wt.% P, 30-50 wt.% Fe, 1-10 wt.% of high-speed tool steel component, 1-5 wt.% of graphite, and 20-55 wt.% copper. COPYRIGHT: (C)2010,JPO&INPIT |