摘要 |
<P>PROBLEM TO BE SOLVED: To provide a low self-shrinkable cement composition of a high pore phase type in which the self-shrinkage is low even when used in a low water cement ratio conventionally causing the self-shrinkage regardless of a high amount of the pore phase, and a large quantity of industrial by-product/industrial waste rich in an Al<SB>2</SB>O<SB>3</SB>component can be used as a cement raw material. Ž<P>SOLUTION: The cement composition containing cement clinker and gypsum is prepared so that the total quantity of C<SB>3</SB>A and C<SB>4</SB>AF is 20-30 mass% and the quantity of f.CaO is 0.28-1 mass%. Ž<P>COPYRIGHT: (C)2010,JPO&INPIT Ž
|
申请公布号 |
JP2010030894(A) |
申请公布日期 |
2010.02.12 |
申请号 |
JP20090234542 |
申请日期 |
2009.10.08 |
申请人 |
MITSUBISHI MATERIALS CORP;UBE IND LTD |
发明人 |
OSAKI MASAFUMI;IGARASHI HIDEAKI;DAIMON SEIKI;SAKAI ETSURO |
分类号 |
C04B7/345 |
主分类号 |
C04B7/345 |