摘要 <p>Constructional elements hardened by thermal treatment or steam-hardening incorporate as binder granulated blast-furnace and steel-making slags. The slags are milled together until specific surface is 3,500-4.500 cm2/g. and the binder contains 40-60% wt. of each of the slags, and opt. 5-10% wt. gypsum or anhydrite. The treated bricks have compression-resistance 172 kPa/cm2.</p>
申请公布号 LU63519(A1) 申请公布日期 1971.11.16
申请号 LUD63519 申请日期 1971.07.13
申请人 发明人
分类号 C04B7/147;C04B40/02 主分类号 C04B7/147