<p>The invention relates to a molten cast refractory material comprising, in oxide wt % and totaling 100%: - ZrO2 + HfO2: the remainder of 100%; - SiO2: 3.5% to 6.0%; - Al2O3: 0.7% to 1.5%; - Na2O + K2O: 0.10 % to 0.43 %; - B2O3: 0.05% to 0.80%; - CaO + SrO + MgO + ZnO: 2O5: 2O3 + TiO2: 2O3/(Na2O + K2O) being greater than or equal to 3.5 and the wt % ratio for B2O3/(Na2O + K2O) being 0.3 to 2.5.</p>
申请公布号
WO2009153517(A1)
申请公布日期
2009.12.23
申请号
WO2009FR51141
申请日期
2009.06.16
申请人
SAINT-GOBAIN CENTRE DE RECHERCHES ET D'ETUDES EUROPEEN;GAUBIL, MICHEL;MASSARD, LUDOVIC