摘要 |
An insulating polymer material composition is obtained by adding an acid anhydride as a curing agent and an organic peroxide such as dicumyl peroxide as a curing accelerator (for example, in an amount of 0.5 to 16.0 phr) to an epoxidized linseed oil, kneading the resulting under conditions according to the added amounts, and then heat-treating the kneaded substance, thereby causing peroxide vulcanization and three-dimensional crosslinking. This insulating polymer material composition is applied to polymer products such as high-voltage devices.
|