摘要 |
PROBLEM TO BE SOLVED: To provide a polyolefinic resin composition having excellent transparency even when a polyolefinic resin having a high melt flow rate (MFR) is used. SOLUTION: The polyolefinic resin composition is obtained by blending a specific dibenzylidene sorbitol compound (A) and an alkali metal salt compound (B) of a specific organophosphate with the polyolefin resin having a melt flow rate (MFR) of≥20 dg/min at 230°C. For 100 pts.mass of the polyolefinic resin, the total amount of the components (A) and (B) is 0.01-1.0 pts.mass, and a ratio (a mass ratio) (A)/(B) of the components (A) to (B) is within the range from 99/1 to 80/20. COPYRIGHT: (C)2010,JPO&INPIT |