发明名称 METHOD FOR INCREASING THE FATIGUE STRENGTH OF A PREDOMINANTLY STEEL MECHANICAL PART OF A WIND TURBINE AND/OR FOR REDUCING THE TENDENCY TO FORM WHAT ARE CALLED WHITE ETCHING CRACKS OR BRITTLE FLAKES IN SUCH STEEL MECHANICAL PARTS
摘要 Method for increasing the fatigue strength of a mechanical part of a wind turbine and/or for reducing the tendency to form what are called "white etching cracks" or "brittle flakes" in such a bearing, characterised in that it consists in making one or several of the bearing rings and/or roller elements concerned of the bearing at least partly of a hardened steel having a carbon content between 0,4 and 0,8 percent by weight.
申请公布号 CA2663736(A1) 申请公布日期 2009.11.20
申请号 CA20092663736 申请日期 2009.04.22
申请人 HANSEN TRANSMISSIONS INTERNATIONAL, NAAMLOZE VENNOOTSCHAP 发明人 BROEDERS, WARD;VAN GEERTSON, JAN;LUYCKX, JOHAN
分类号 C21D1/00;C21D1/09;C21D1/10;C21D9/32;C21D9/40;C22C38/00 主分类号 C21D1/00