发明名称 ARAMID TIRE CORD AND MANUFACTURING METHOD THEREOF
摘要 The present invention relates to an aramid tire cord with a superior initial modulus change rate, a tensile strain and an initial modulus, and a manufacturing method thereof. The present invention provides an aramid tire cord containing an aramid multi-filament, wherein the initial modulus change rate after repetitive stretch tests performed at 10 times the load of 10% of the cutting strength at 120?, is 5% or lower, and a manufacturing method thereof. The aramid tire cord of the present invention exhibits an excellent initial modulus change rate, a tensile strain and an initial modulus retention at a high temperature, and thus has an excellent fatigue resistance as the aramid tire cord has an optimum modulus and a crystallization constant value and a crystallization orientation constant. Accordingly, the aramid tire cord of the present invention prevents degradation of physical properties and improves travel performance even under high speed travel for long durations with a high temperature and high pressure conditions, when the aramid tire cord is used as a reinforcement material for a tire.
申请公布号 WO2009134063(A2) 申请公布日期 2009.11.05
申请号 WO2009KR02232 申请日期 2009.04.28
申请人 KOLON INDUSTRIES, INC.;KWON, SO YEON 发明人 KWON, SO YEON
分类号 D02G3/48;D01F6/60 主分类号 D02G3/48
代理机构 代理人
主权项
地址