METHOD FOR SYNTHESIZING METAL NANOPARTICLE |
摘要 |
PROBLEM TO BE SOLVED: To synthesize metal nanoparticles which do not contain a corrosive material, from an insoluble metal salt, and to produce the metal nanoparticles which are preferably used for an electrically conductive material. SOLUTION: The method for synthesizing the metal nanoparticles includes the steps of: preparing an aqueous solution A of the metal salt by dissolving the metal salt in water; preparing an aqueous solution B of a carboxylic acid by dissolving a compound such as glycolic acid in water; preparing an aqueous solution C of a reducing agent; preparing a basic aqueous solution D; producing a mixture solution by adding the aqueous solution A of the metal salt dropwise into the basic aqueous solution D while stirring the mixed product; producing a suspension of the carboxylate by adding the aqueous solution B of the carboxylic acid dropwise into the mixture solution while stirring the mixed product; and producing the metal nanoparticle by adding the aqueous solution C of the reducing agent dropwise into the suspension of the carboxylate while stirring the mixed product. Metal elements contained in the metal salt contain 75 wt.% or more silver. In the step of producing the metal nanoparticle by adding the aqueous solution C of the reducing agent dropwise, the mixed product is stirred at a temperature of 25 to 95°C. COPYRIGHT: (C)2010,JPO&INPIT |
申请公布号 |
JP2009221600(A) |
申请公布日期 |
2009.10.01 |
申请号 |
JP20090003471 |
申请日期 |
2009.01.09 |
申请人 |
MITSUBISHI MATERIALS CORP |
发明人 |
YAMAZAKI KAZUHIKO;SENGOKU AIRI;ARAI MASAHIDE;HAYASHI TOSHIHARU |
分类号 |
B22F9/24;B22F9/00;C22C5/06;H01B13/00 |
主分类号 |
B22F9/24 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|