发明名称 Natural rubber mixture with improved low temperature flexibility
摘要 <p>Rubber mixture comprises at least a solid diene rubber (30-100 parts per hundred (phr)); at least a low viscous and liquid rubber; at least a thiuram catalyst (0.1-10); at least an amorphous and/or precipitated silicic acid (0-150 phr); at least a coupling agent (0-25 phr); at least a soot (1-100 phr); and a further additive (2-200 phr).</p>
申请公布号 EP2082899(A1) 申请公布日期 2009.07.29
申请号 EP20080171878 申请日期 2008.12.17
申请人 CONTINENTAL REIFEN DEUTSCHLAND GMBH 发明人 WEINREICH, HAJO, DR.
分类号 B60C1/00;C08K3/04;C08K3/06;C08K3/36;C08K5/40;C08L9/00;C08L21/00 主分类号 B60C1/00
代理机构 代理人
主权项
地址