发明名称 CONCRETE OPTIMIZED FOR HIGH WORKABILITY AND HIGH STRENGTH TO CEMENT RATIO
摘要 <p>A concrete composition having a 28-day design compressive strength of 4000 psi and a slump of about 5 inches is optimized to have high workability and a high strength to cement ratio. The concrete composition contains about 375 pounds per cubic yard hydraulic cement (e.g., Portland cement), about 113 pounds per cubic yard pozzolanic material (e.g., Type C fly ash), about 1735 pounds per cubic yard fine aggregate (e.g., FA-2 sand), about 1434 pounds per cubic yard coarse aggregate (e.g., CA-li state rock, 3/4 inch), and about 294 pounds per cubic yard water (e.g., potable water). Workability and strength to cement ratio were increased compared to one or more preexisting concrete compositions having the same 28-day design compressive strength and similar slump by optimizing the ratio of fine aggregate to coarse aggregate. The concrete composition is further characterized by high cohesiveness, resulting in relatively little or no segregation or bleeding.</p>
申请公布号 WO2009085435(A1) 申请公布日期 2009.07.09
申请号 WO2008US83905 申请日期 2008.11.18
申请人 ICRETE LLC;ANDERSEN, PER JUST;HODSON, SIMON K. 发明人 ANDERSEN, PER JUST;HODSON, SIMON K.
分类号 C04B28/00;C04B14/00 主分类号 C04B28/00
代理机构 代理人
主权项
地址