PROBLEM TO BE SOLVED: To provide a polyethersulfone-based resin composition having a low outgassing property and melt processability at high levels and a molding obtained by using the polyethersulfone-based resin composition. SOLUTION: The polyethersulfone-based resin composition is obtained by melt-kneading 100 parts weight polyethersulfone resin (A) and 1-20 parts weight low-molecular compound (B) which has≥150°C start temperature of weight loss, when measured according to JIS K7120,≥100°C melting point and≤500 molecular weight. The molding excellent in low outgassing property is obtained from the polyethersulfone-based resin composition. COPYRIGHT: (C)2009,JPO&INPIT
|