The invention relates to the use of polyalkyl(meth)acrylate bead polymers with an average particle size V50 that ranges between 30 and 70 mum for improving the stress cracking resistance of moulding materials containing polyalkyl(meth)acrylate. The invention also relates to moulding materials comprising: a) at least 50 wt. % of an impact resistance modifying agent, which contains at least one polyalkyl(meth) acrylate phase; b) at least 8 wt. % of a polyalkyl(meth)acrylate bead polymer with an average particle size V50 that ranges between 30 and 70 mum; and c) between 0 and 42 wt. % of a polyalkyl(meth)acrylate with a molecular weight ranging between 20,000 and 350,000 g/mol, whereby the wt. % of the components a) to c) amounts to 100 wt. %, and to moulded bodies that can be obtained from said materials.
|