摘要 |
A method for preparing an electrode material for battery is provided. The method includes the following steps: firstly, providing a reaction precursor having a crystal structure, in which the reaction precursor represents as NaxMyM'zO2, and M and M' are not the same metal; next, dispersing the reaction precursor in a solvent, and adding a lithium (Li) salt therein, so as to form a mixed solution; and then, performing a microwave heating treatment on the mixed solution, in which Li+ in the Li salt are ion exchanged with Na+ in the reaction precursor, so as to form LixMyM'zO2 as the electrode material.
|