发明名称 |
Process for the manufacture of a fibre reinforced material consisting at least on the peripheral area of a metal-ceramic composite material |
摘要 |
<p>The fiber-reinforced composite material comprises fibers, surface layer and matrix. The matrix contains silicon carbide (at least 25 weight%) and phases of silicon, silicon alloys and/or carbon, and has a structure containing open cracks and/or pores. Metal(s) are deposited at least in some open cracks or pores in the matrix structure. Independent claims are included for: (i) molding comprising the fiber-reinforced composite material; (ii) brake disk; (iii) brake lining; (iv) clutch plate; (v) method for producing the fiber-reinforced material; and (vi) method for producing molding.</p> |
申请公布号 |
EP1273817(B1) |
申请公布日期 |
2009.05.06 |
申请号 |
EP20020012959 |
申请日期 |
2002.06.12 |
申请人 |
AUDI AG |
发明人 |
CHRIST, MARTIN, DR.;HEINE, MICHAEL, DR.;KIENZLE, ANDREAS, DR.;ZIMMERMANN-CHOPIN, RAINER, DR. |
分类号 |
F16D69/02;C04B35/571;C04B35/573;C04B35/628;C04B35/80;C04B35/83;C04B41/51;C04B41/52;C04B41/88;C04B41/89;F16D65/12 |
主分类号 |
F16D69/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|