发明名称
摘要 <p>In one embodiment the invention is an article comprising at least two layers, a first or low crystallinity layer comprising a low crystallinity polymer and a second or high crystallinity layer comprising a high crystallinity polymer. The high crystallinity polymer has a melting point as determined by differential scanning calorimetry (DSC) that is about the same or within less than 25 C of the melting point of the low crystallinity polymer. The article is elongated at a temperature below the melting point of the low crystallinity polymer in at least one direction to an elongation of at least about 50% of its original length or width, to form a pre-stretched article. Preferably, the high crystallinity layer is capable of undergoing plastic deformation upon the elongation.</p>
申请公布号 JP2009513395(A) 申请公布日期 2009.04.02
申请号 JP20080538147 申请日期 2006.10.24
申请人 发明人
分类号 B32B27/00;A61F13/49;A61F13/496;A61F13/514;B32B5/26;B32B27/32;D04H1/42 主分类号 B32B27/00