摘要 |
<P>PROBLEM TO BE SOLVED: To provide a glass frit which provides a good sealing effect to moisture and gas and is processable at low temperature, and a sealing method for an electric element using the same. <P>SOLUTION: Disclosed is a glass frit comprising, by mol, 10 to 25% P<SB>2</SB>O<SB>5</SB>, 40 to 50% V<SB>2</SB>O<SB>5</SB>, 10 to 20% ZnO, 1 to 15% BaO, 1 to 10% Sb<SB>2</SB>O<SB>3</SB>, 1 to 10% Fe<SB>2</SB>O<SB>3</SB>, 0.1 to 5% Al<SB>2</SB>O<SB>3</SB>, 0.1 to 5% B<SB>2</SB>O<SB>3</SB>, 1 to 10% Bi<SB>2</SB>O<SB>3</SB>and 0.1 to 5% TiO<SB>2</SB>. <P>COPYRIGHT: (C)2009,JPO&INPIT |