摘要 |
<p>The invention relates to a method for producing a strip-cast, low-carbon, partly Mn/Si killed steel strip that is largely free of cracks and surface defects from a steel melt with a sulphur content of between 20 and 300 ppm and an Mn/Si ratio â¿¥ 3.5, using a strip forming force of between 2 and 50 kN/m.</p> |