摘要 |
PROBLEM TO BE SOLVED: To provide a method for efficiently producing, without blending, a rubber-modified styrenic resin suitably used for large-size blow molding which is free from a gelled product and has an excellent physical property balance among flowing property, melt tension and impact resistance, and a resin composition obtained by the method. SOLUTION: The method for producing the rubber-modified styrenic resin composition comprises using, based on 100 pts.wt. in total of an aromatic monovinyl compound and a rubber-like component, 30×10<SP>-4</SP>to 160×10<SP>-4</SP>pts.wt. of a polyfunctional vinyl compound, 50×10<SP>-4</SP>to 260×10<SP>-4</SP>pts.wt. of a polymerization initiator, and 100×10<SP>-4</SP>to 2000×10<SP>-4</SP>pts.wt. of silicone oil. COPYRIGHT: (C)2009,JPO&INPIT
|