发明名称 STRENGTHENED IRON CATALYST FOR SLURRY REACTORS
摘要 <p>A method of strengthening a precipitated unsupported iron catalyst by: preparing a precipitated unsupported iron catalyst containing copper and potassium; adding a solution comprising a structural promoter to the previously prepared catalyst; drying the mixture; and calcining the dried catalyst. A method for preparing an iron catalyst, the method comprising: precipitating a catalyst precursor comprising iron phases selected from hydroxides, oxides, and carbonates; adding a promoter to the catalyst precursor to yield a promoted precursor; drying the promoted precursor to yield dried catalyst; and calcining the dried catalyst, wherein the catalyst further comprises copper and potassium. A method of preparing a strengthened precipitated iron catalyst comprising: co-precipitating iron, copper, magnesium, and aluminum; washing the precipitate; alkalizing the precipitate; and drying the precipitate to yield a dried catalyst precursor. The dried catalyst precursor may be calcined and treated with a gas comprising carbon monoxide.</p>
申请公布号 WO2009032701(A2) 申请公布日期 2009.03.12
申请号 WO2008US74484 申请日期 2008.08.27
申请人 RENTECH, INC.;BENHAM, CHARLES, B.;FRAENKEL, DAN;BLEY, RICHARD, A.;TAYLOR, JESSE, W.;DEMIREL, BELMA;ROLFE, SARA, L.;WRIGHT, HAROLD, A. 发明人 DEMIREL, BELMA;ROLFE, SARA, L.;WRIGHT, HAROLD, A.
分类号 B01J23/78;C07C27/06 主分类号 B01J23/78
代理机构 代理人
主权项
地址