发明名称 |
STRENGTHENED IRON CATALYST FOR SLURRY REACTORS |
摘要 |
A method of strengthening a precipitated unsupported iron catalyst by: preparing a precipitated unsupported iron catalyst containing copper and potassium; adding a solution comprising a structural promoter to the previously prepared catalyst; drying the mixture; and calcining the dried catalyst. A method for preparing an iron catalyst, the method comprising: precipitating a catalyst precursor comprising iron phases selected from hydroxides, oxides, and carbonates; adding a promoter to the catalyst precursor to yield a promoted precursor; drying the promoted precursor to yield dried catalyst; and calcining the dried catalyst, wherein the catalyst further comprises copper and potassium. A method of preparing a strengthened precipitated iron catalyst comprising: co-precipitating iron, copper, magnesium, and aluminum; washing the precipitate; alkalizing the precipitate; and drying the precipitate to yield a dried catalyst precursor. The dried catalyst precursor may be calcined and treated with a gas comprising carbon monoxide.
|
申请公布号 |
CA2698123(A1) |
申请公布日期 |
2009.03.12 |
申请号 |
CA20082698123 |
申请日期 |
2008.08.27 |
申请人 |
RENTECH, INC. |
发明人 |
DEMIREL, BELMA;ROLFE, SARA L.;WRIGHT, HAROLD A.;BENHAM, CHARLES B.;FRAENKEL, DAN;BLEY, RICHARD A.;TAYLOR, JESSE W. |
分类号 |
B01J23/78;C07C27/06 |
主分类号 |
B01J23/78 |
代理机构 |
|
代理人 |
|
主权项 |
|