摘要 FIELD: chemistry, construction. ^ SUBSTANCE: binding agent includes, wt %: semi-water gypsum of beta-modification -57.3-62.9, grinded basic granular blast-furnace slag - 15.2-16.25, caustic magnesite - 10.8-16.25, clyite dust from cyclones - 0.45-0.9, bischofite solution with density 1.2 g/cm3 in terms of magnesium chloride MgCl2 -9.75-10.2. Method of preparation of said binding agent includes mixing said gypsum, said slag and caustic magnesite, tempering of dry mixture with bischofite solution with density 1.2 g/cm3 and further introduction of said dust 1-2 min before formation. ^ EFFECT: increase of strength under compression, extension of stiffening terms, reduction of binding agent water resistance. ^ 2 cl, 2 tbl
申请公布号 RU2341477(C1) 申请公布日期 2008.12.20
申请号 RU20070111867 申请日期 2007.03.30
申请人 GOSUDARSTVENNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA TUL'SKIJ GOSUDARSTVENNYJ UNIVERSITET (TULGU) 发明人 RJABOV GENNADIJ GAVRILOVICH;MISHUNINA GALINA EVGEN'EVNA;RJABOV ROMAN GENNAD'EVICH;ZABRODINA NADEZHDA IVANOVNA
分类号 C04B11/30 主分类号 C04B11/30
代理机构 代理人
主权项
地址