摘要 |
PROBLEM TO BE SOLVED: To provide a covering material having excellent processability and high reflectivity. SOLUTION: The covering material is produced by coating with an acrylic paint comprising (A) 10-90 pts.mass of an amorphous polyester having a number-average molecular weight of 1,000-40,000, a glass transition temperature of -20 to +60°C and a specific gravity of≤1.23 at 30°C, (B) 90-10 pts.mass of a (meth)acrylic monomer and (C) titanium oxide, wherein the (meth)acrylic monomer (B) contains a compound expressed by general formula (1), and the amount of the compound is 10-50 mol% in the total (meth)acrylic monomer. COPYRIGHT: (C)2009,JPO&INPIT
|