发明名称 Method for controlling bright annealing furnace
摘要 The steam partial pressure of the internal environment within a bright annealing furnace generating a boron oxide is reduced to less than about 1x10<SUP>-5 </SUP>by lowering the dew point of the internal furnace environment. The dew point of the heating environment within the bright annealing furnace is lowered by introducing a gas having a hydrocarbon component or a chemical compound having a carbon component into the furnace.
申请公布号 US2007107817(A1) 申请公布日期 2007.05.17
申请号 US20040574637 申请日期 2004.10.12
申请人 CHUGAI RO CO., LTD. 发明人 KOUSAKA KENJI;IMADA MORIHIKO
分类号 C21D1/76 主分类号 C21D1/76