发明名称 Carbon black with large primary particle size as reheat additive for polyester and polypropylene resins
摘要 Reheat characteristics of polyethylene and polypropylene resins, including reheating time and resin color, are improved by adding to the resin carbon black with a primary particle size in the range of 200 to 500 nm as an infrared absorber. Thermal carbon blacks having this primary particle size are preferred over Furnace carbon blacks. Injection stretch-blow molded bottles and other thermoformed products are made from resins with carbon black infrared absorber.
申请公布号 US2006099364(A1) 申请公布日期 2006.05.11
申请号 US20040984506 申请日期 2004.11.08
申请人 INVISTA NORTH AMERICA S.A.R.L. 发明人 HARRISON DAVID A.;DAVIS J. P.
分类号 B32B27/08 主分类号 B32B27/08