发明名称 MIXED SLURRY FOR SOLDERING ALUMINUM ALLOY, AND METHOD FOR MANUFACTURING SANDWICH PANEL USING THE SAME
摘要 PROBLEM TO BE SOLVED: To provide soldering slurry which can carry out soldering at a low temperature and is inexpensive, and further to provide an aluminum alloy sandwich panel which has been soldered using the same soldering slurry, and is light-weighted, has an excellent appearance, and is inexpensive. SOLUTION: Mixed slurry for soldering an aluminum alloy contains a soldering material composed of a powder aluminum alloy having an average grain diameter of 10 to 100μm, which powder aluminum alloy has been manufactured by spraying and quenching the molten metal of the aluminum alloy containing 23 to 37 mass% of Cu and 4 to 10 mass% of Si in a vacuum or an inert gas, and a fluoride flux including 11 mass% or more of CsF as a solid component. The aluminum alloy sandwich panel is formed by soldering face plate materials 2 and core materials 3 using the mixed slurry for soldering. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP2006116551(A) 申请公布日期 2006.05.11
申请号 JP20040303969 申请日期 2004.10.19
申请人 NIPPON LIGHT METAL CO LTD 发明人 OKI YOSHITO;SASAKI TOMOHIRO;KURAMASU YUKIO
分类号 B23K35/22;B22F1/00;B22F9/08;B23K1/00;B23K1/19;B23K31/02;C22C21/00 主分类号 B23K35/22
代理机构 代理人
主权项
地址