摘要 |
PROBLEM TO BE SOLVED: To obtain an injection molded article excellent in the balance of heat resistance, appearance, low warpage, and scratch resistance. SOLUTION: This injection molded article is obtained by molding a thermoplastic resin composition comprising 20 to 60 pts.wt. of a styrenic resin (A) having an unsaturated nitrile monomer content of 32 to 50 mass% in an acetone-soluble component, 20 to 60 pts.wt. of an aromatic polyester (B) having an isothermal crystallization time of 20 to 100 sec from a melted state, and 20 to 60 pts.wt. of a filler (C) with a mold whose surface highest site temperature is 80 to 120°C. COPYRIGHT: (C)2008,JPO&INPIT |