发明名称 |
IMPROVED ATMOSPHERIC-PRESSURE ALUMINIUM BRAZING METHOD |
摘要 |
The present invention relates to an aluminium brazing method conducted in an atmospheric-pressure furnace, which is characterized by the implementation of the following operational conditions: i) the filler alloy used is an alloy obtained by mechanical synthesis, comprising aluminium, silicon, nickel and optionally magnesium or other alloying elements, such as copper, zinc, silver, chromium and titanium; j) the oxygen content in the furnace is less than a few ppm, preferably less than 1 ppm and that the dew point in the furnace is below -30°C, preferably below -40°C and even more preferably still below -45°C. |
申请公布号 |
WO2008148986(A2) |
申请公布日期 |
2008.12.11 |
申请号 |
WO2008FR50782 |
申请日期 |
2008.05.02 |
申请人 |
CENTRE REGIONAL D'INNOVATION ET DE TRANSFERT DE TECHNOLOGIE POUR LA TRANSFORMATION ET LE TRAITEMENTDES METAUX ET ALLIAGES (CRITT);L'AIR LIQUIDE SOCIETE ANONYME POUR L'ETUDE ET L'EXPLOITATION DES PROCEDES GEORGES CLAUDE;MAZET, THIERRY;JULLIARD, FRANCK;RIDLOVA, MARTINA;DULCY, JACKY;GANTOIS, MICHEL |
发明人 |
MAZET, THIERRY;JULLIARD, FRANCK;RIDLOVA, MARTINA;DULCY, JACKY;GANTOIS, MICHEL |
分类号 |
B23K1/008;B23K1/19;C01B21/04 |
主分类号 |
B23K1/008 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|