发明名称 METHOD OF OBTAINING FINE CRYSTALLINE ALLOYED LANTHANUM ALUMINATE
摘要 FIELD: chemistry. ^ SUBSTANCE: mixture of aluminum hydroxide, lanthanum oxide and alloying additives is subjected to thermal processing in water vapour in autoclave in two stages. First stage is carried out in temperature interval 180-250C, and the second - in temperature interval 390-450C. As alloying additives oxides or salts of elements, selected from line: Mg, Cr, Eu, Ce in amount from 0.001 to 2% weight from lanthanum aluminate weight are used. ^ EFFECT: obtaining lanthanum aluminate with low water content, alloyed, magnesium, chrome, europium or cerium. ^ 3 dwg, 6 ex
申请公布号 RU2340558(C2) 申请公布日期 2008.12.10
申请号 RU20060147175 申请日期 2006.12.29
申请人 DANCHEVSKAJA MARINA NIKOLAEVNA;IVAKIN JURIJ DMITRIEVICH;TORBIN SERGEJ NIKOLAEVICH 发明人 DANCHEVSKAJA MARINA NIKOLAEVNA;IVAKIN JURIJ DMITRIEVICH;TORBIN SERGEJ NIKOLAEVICH
分类号 C01F7/04;C01F17/00 主分类号 C01F7/04