发明名称 HEAT-RESISTANT ALUMINUM ALLOY
摘要 PROBLEM TO BE SOLVED: To provide an aluminum alloy with good thermal stability for the production of thermally and mechanically stressed cast components. SOLUTION: The aluminum alloy contains 11.0-12.0 wt.% silicon, 0.7-2.0 wt.% magnesium, 0.1-1 wt.% manganese, at most 1 wt.% iron, at most 2 wt.% copper, at most 2 wt.% nickel, at most 1 wt.% chromium, at most 1 wt.% cobalt, at most 2 wt.% zinc, at most 0.25 wt.% titanium, 40 ppm boron, optionally 80-300 ppm strontium, and aluminum as the reminder with further elements and impurities due to production individually at most 0.05 wt.%, in total at most 0.2 wt.%. COPYRIGHT: (C)2009,JPO&INPIT
申请公布号 JP2008291364(A) 申请公布日期 2008.12.04
申请号 JP20080133893 申请日期 2008.05.22
申请人 ALUMINIUM RHEINFELDEN GMBH 发明人 DRAGULIN DAN;FRANKE RUEDIGER
分类号 C22C21/02;B22D17/00;C22F1/00;C22F1/043 主分类号 C22C21/02