发明名称 Ni-Cr BASE ALLOY WITH EXCELLENT RESISTANCE TO NITRIC-HYDROFLUORIC ACID CORROSION
摘要 PROBLEM TO BE SOLVED: To provide an Ni-Cr base alloy having more excellent corrosion resistance to an aqueous solution of nitric-hydrofluoric acid. SOLUTION: The alloy has a composition which consists of >43 to 47% Cr, 0.01 to 2% Mo, 0.05 to 1% Fe, 0.01 to 0.1% Si, 0.01 to 0.2% V, 0.001 to 0.05% Mg, 0.001 to 0.04% N, 0.05 to 0.5% Mn and the balance Ni with inevitable impurities and further contains, if necessary, one or more kinds among (i) 0.01 to 2% Cu, (ii) 0.01 to 0.2%, in total, of either or both of Al and Ti and (iii) 0.0005 to 0.01% B and in which the amount of C contained as an inevitable impurity is regulated to≤0.05%. COPYRIGHT: (C)2009,JPO&INPIT
申请公布号 JP2008291281(A) 申请公布日期 2008.12.04
申请号 JP20070134900 申请日期 2007.05.22
申请人 MITSUBISHI MATERIALS CORP 发明人 SAKAI HIROKAZU;SUGAWARA KATSUO
分类号 C22C19/05;C22F1/00;C22F1/10;F28F21/08;H01L21/306 主分类号 C22C19/05