发明名称 TOOTH FLUORIDATING AND REMINERALIZING COMPOSITIONS AND METHODS, BASED ON NANOAGGREGATE FORMATION
摘要 Compositions and methods for forming, in an aqueous environment, a nanoaggregate of calcium fluoride and amorphous calcium phosphate-containing compound, such as amorphous calcium phosphate fluoride or amorphous calcium carbonate phosphate fluoride are described. The nanoaggregate (or nanocomposite) can release calcium, phosphate, and fluoride, and ultimately convert to the tooth mineral, fluorapatite. One method for forming such a nanoaggregate involves applying a non-aqueous (e.g., varnish-based) composition (e.g., a suspension), containing solid particles of water soluble salts of calcium, phosphate, and fluoride, to the aqueous environment of the mouth. This results in rapid solubilization of the salts, precipitation of the nanoaggregate, and tooth remineralization. Tooth fluoridation and remineralization may also be carried out by applying to the tooth a non-aqueous carrier containing the nanoaggregate. Whitening agents can also be added to these compositions and methods.
申请公布号 US2008292565(A1) 申请公布日期 2008.11.27
申请号 US20080126426 申请日期 2008.05.23
申请人 ADA FOUNDATION 发明人 TUNG MING S.
分类号 A61K8/24 主分类号 A61K8/24
代理机构 代理人
主权项
地址