发明名称 |
method of obtaining the hard alloys |
摘要 |
A method of obtaining the hard alloys includes pressing of charge, sintering at heating at a rate of 35-40 deg./ min. to 800-850 °C with subsequent soaking during 30-40 min., and then is accomplished the heating at a rate of 50-55 deg./ min. to the temperature of liquid-phase sintering with subsequent soaking. After heating to the temperature of liquid-phase sintering the soaking during 3-20 min. is carried out, while after this temperature is reduced down to the temperature of solid-phase sintering of 1200-1250 °C and is achieved soaking during 60-120 min. |
申请公布号 |
UA37244(U) |
申请公布日期 |
2008.11.25 |
申请号 |
UA20080006401U |
申请日期 |
2008.05.14 |
申请人 |
BAKUL INSTITUTE OF SUPERHARD MATERIALS OF THE NATIONAL ACADEMY OF SCIENCES OF UKRAINE;KHARCHENKO OLEH VALENTYNOVYCH;PROKOPIV NAZAR MYKOLAIOVYCH |
发明人 |
PROKOPIV MYKOLA MYKHAILOVYCH;KHARCHENKO OLEH VALENTYNOVYCH;PROKOPIV NAZAR MYKOLAIOVYCH |
分类号 |
B22F3/12;C22C1/05 |
主分类号 |
B22F3/12 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|