A method of producing a PCD body includes the step of providing a region of coarser diamond particles between a source of binder phase and a region of fine grained diamond particles having a particle size less than 2 µm. The binder phase is caused to infiltrate the diamond mass through the region of coarser diamond particles under elevated temperature and pressure conditions suitable to produce PCD. The invention further provides for a PCD diamond composite manufactured by the method of the invention wherein the PCD body is substantially free of abnormal diamond growth.
申请公布号
WO2008135949(A2)
申请公布日期
2008.11.13
申请号
WO2008IB51749
申请日期
2008.05.06
申请人
ELEMENT SIX (PRODUCTION) (PTY) LTD;DAVIES, GEOFFREY JOHN;PETERS, GERRARD