摘要 |
<P>PROBLEM TO BE SOLVED: To provide a cellulose acylate film superior in conveying properties even at a high temperature, and satisfactory in surface state even after heat treatment. <P>SOLUTION: The cellulose acylate film satisfies formulae (I) and (II). The formula (I) is 1.01≤E'(//)/E'(⊥)≤1.30 and the formula (II) is 5≤σ<SB>240</SB>(20%)≤100, wherein E'(//) is a tensile elastic modulus (unit; MPa) in a direction in which the tensile elastic modulus (unit; MPa) becomes maximum at 25°C in the plane, E'(⊥) is tensile elastic modulus (unit; MPa) in a direction crossing the measuring direction of E'(//) at right angles, and σ<SB>240</SB>expresses a tensile stress (unit; N/mm<SP>2</SP>) when being stretched 20% at 240°C in a direction in which the tensile elastic modulus at 25°C becomes maximum in the plane. <P>COPYRIGHT: (C)2009,JPO&INPIT |