发明名称 Method for making mineral wool, cobalt-based alloys therefor and other uses
摘要 <p>The invention concerns a method for making mineral wool by internal centrifuging characterised in that the temperature of the mineral material in the fibre-forming spinner is at least 1100 °C and the fibre-forming spinner consists of a cobalt-based alloy comprising the following elements (in weight percentages of the alloy): Cr 23 to 34 %, Fe less than 3 %, Ni 6 to 12 %, Si less than 1 %, Ta 3 to 10 %, Mn less than 0.5 %, C 0.2 to 1.2 %, Zr less than 0.1 %, W 0 to 8 %, the rest being formed by cobalt and unavoidable impurities, the mol ratio of tantalum to carbon being at least 0.3. The invention also concerns alloys particularly suited for this method corresponding to said formula and do not contain tungsten. The inventive alloys can be used for other purposes in oxidising atmosphere at a temperature of at least 1100 °C.</p>
申请公布号 SK286499(B6) 申请公布日期 2008.11.06
申请号 SK20020001627 申请日期 2001.05.23
申请人 SAINT-GOBAIN ISOVER 发明人 BERTHOD PATRICE;BERNARD JEAN LUC;LIEBAUT CHRISTOPHE
分类号 C22F1/10;C03B37/04;C03B37/095;C22C19/07;C22F1/00;D01F9/08 主分类号 C22F1/10
代理机构 代理人
主权项
地址
您可能感兴趣的专利