发明名称 |
METHOD FOR PRODUCING ROLLING BEARING CONSTITUTING MEMBER, AND ROLLING BEARING |
摘要 |
PROBLEM TO BE SOLVED: To prolong the service life of a rolling bearing by restraining the breakage of the inner starting point. SOLUTION: An inner ring 1 and an outer ring 2 are produced by using steel satisfying equation (2) in the relation of DI value indicated with equation (1) and the thickness t(mm). (1) DI=(0.2[C]+0.128)(1+0.7[Si])(1+3.45[Mn])(1+0.07[Ni]+0.27[Ni][Ni])(1+2[Cr])(1+2.5[Mo])(1+0.35[Cu]). (2) DI/t≥0.45. COPYRIGHT: (C)2009,JPO&INPIT
|
申请公布号 |
JP2008266683(A) |
申请公布日期 |
2008.11.06 |
申请号 |
JP20070108343 |
申请日期 |
2007.04.17 |
申请人 |
NSK LTD |
发明人 |
WATANUKI DAISUKE;TOBITAKA HIDEYUKI;MITSUYASU YUTARO |
分类号 |
C21D9/40;C21D1/06;C22C38/00;C22C38/44;C23C8/22;C23C8/32;F16C33/32;F16C33/34;F16C33/62 |
主分类号 |
C21D9/40 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|