发明名称 HYDRAULIC COMPOSITION
摘要 <p><P>PROBLEM TO BE SOLVED: To provide a hydraulic composition which exhibits excellent flowability, nonshrinking property, and strength after being hardened, in various grouting (injection) methods in the civil engineering and construction field without using mineral matter fine powders such as waste fly ash, blast furnace slag, or the like and spherical aggregate, and which has flowability enough to be suitably filled into a joint sleeve for joining reinforcing bar and nonshrinking property for firmly unifying a construction region and is excellent in strength characteristics of a hardened body, in particular in a construction method for joining precast reinforced concrete members at a field. <P>SOLUTION: The hydraulic composition contains cement and a fine aggregate containing a ferronickel slag, wherein the ferronickel slag is characterized by containing particles having a particle size of 0.075-2.4 mm of 80 mass% or more and particles having a particle size less than 0.075 mm of less than 10 mass% in 100 mass% ferronickel slag. <P>COPYRIGHT: (C)2009,JPO&INPIT</p>
申请公布号 JP2008260672(A) 申请公布日期 2008.10.30
申请号 JP20070241359 申请日期 2007.09.18
申请人 UBE IND LTD 发明人 ARAI KAZUYA;HIRANO YOSHINOBU;OKADA YUKIHIKO;OSHIMA MASANORI
分类号 C04B28/02;C04B18/14;C04B22/04;C04B22/06;C04B24/26;C04B24/32;C04B24/38;C04B111/70 主分类号 C04B28/02
代理机构 代理人
主权项
地址