摘要 |
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having less environmental load and many characteristics advantageous for the use for a long period of time, a thermoplastic resin molded product and a method for manufacturing the molded product. SOLUTION: This thermoplastic resin composition comprises a styrene resin of 1-98 pts.wt., an aliphatic polyester resin of 1-80 pts.wt., and a vinyl polymer of 1-80 pts.wt. (wherein, the total of the styrene resin, the aliphatic polyester resin and the vinyl polymer is 100 pts.wt.). The thermoplastic resin molded product is obtained by molding the heated and melted thermoplastic resin composition. The method for manufacturing the thermoplastic resin molded product that is molded by heating and melting the thermoplastic resin composition or the thermoplastic resin molded product is also disclosed. COPYRIGHT: (C)2009,JPO&INPIT
|