摘要 A plated steel wire having a plated layer and an intermediate layer is characterized in that a content of manganese contained in both the plated layer and the intermediate layer is 0.02-0.30% in terms of average mass percentage, a content of aluminum is 8-25% in terms of average mass percentage, and a content of zinc and inevitable components is 74.70-91.98% in terms of average mass percentage, and that a total deposition amount of the intermediate layer and the plated layer per unit area of the steel wire surface is set to 700-1000 g/m2. The plated steel wire has excellent corrosion resistance and excellent workability, with the increased total deposition amount of the plated layer and the intermediate layer.